Effect of Aluminum Casting Dross Addition on Mechanical Properties and Microstructure in Aluminum Foam Production

Yükleniyor...
Küçük Resim

Tarih

Dergi Başlığı

Dergi ISSN

Cilt Başlığı

Yayıncı

TUBITAK

Erişim Hakkı

info:eu-repo/semantics/openAccess

Özet

In the study, Al foams were produced using 6063 Al alloy casting dross and Boric acid. Foam materials were sintered at 130 ºC for 1 hour and at 550 ºC for 3 hours. The microstructure was analyzed with optical and scanning electron microscopes (SEM). Compression strength was measured with a compression tester. The porosity increased from 34.8% to 37.8%, the compressive strength increased from 12.43 MPa to 20.25 MPa, and the hardness increased from 98 HV to 115 HV with increasing dross amount. © 2022, TUBITAK. All rights reserved.

Açıklama

Anahtar Kelimeler

Aluminum Foam, Characterization, Compressive Strength, Dross

Kaynak

El-Cezeri Journal of Science and Engineering

WoS Q Değeri

Scopus Q Değeri

Cilt

9

Sayı

3

Künye

Onay

İnceleme

Ekleyen

Referans Veren